by Administrator | Feb 25, 2018 | Uncategorized
In order to be able to run more plates and become more efficient in the long run, Beckman decided to install the SEAL Kit Software onto another computer. Because it took time, it was too late to run any plates this week. After researching and looking through previous...
by Administrator | Feb 21, 2018 | Uncategorized
Beckman Group 1 created a sodium sulfite solution for testing. Because the epoxy has proven to be weaker when being put into the testing solution after five to ten minutes of drying, they are waiting for 45 minutes for it to dry before testing. Group 2 is testing a...
by Administrator | Feb 12, 2018 | Uncategorized
It’s been a slow few weeks so I combined the updates into one post. Poly tested two MnCaO and two MnVO plates but didn’t report on the results (not good?). They also wanted to try a different method of pre-cleaning plates to allow for better results, so...